Mario, Even though this is a rejectable condition, with the customers blessing we have MRB'd (agreed between Mfg, Quality and Eng.) that this is a usable condition on many occasions. The conformal coat will more that protect the area from corrosion concerns and will also isolate the area. BS Mario Dion <mdion@MEDIAT To: [log in to unmask] RIX.COM> cc: Sent by: Subject: Re: [TN] Assembled pcb with exposed copper; is TechNet conf.coating appropriate to "isolate" the exposed <[log in to unmask] copper ? ORG> 11/07/2003 09:11 AM Please respond to "TechNet E-Mail Forum."; Please respond to Mario Dion Bonjour Leo, Thanks for your input. I was aware that it is a rejectable condition but since there is $$$ involved if we have to scrap the ccas then that explain why I was looking for a viable solution. By the way, my house is brand new so I can't check for the copper plumbing which anyway are made out of plastic tubbing... ;o) See you in Amherst on December ! Have a great week end all, Mario -----Original Message----- From: Leo Lambert [mailto:[log in to unmask]] Sent: 7 novembre, 2003 09:00 To: TechNet E-Mail Forum.; Mario Dion Subject: RE: [TN] Assembled pcb with exposed copper; is conf.coating appropriate to "isolate" the exposed copper ? Interesting, the boards are hot air leveled (HAL), if inspected to IPC-A-600, sect 2.4.1 Nonwetting, states that this is a non conforming condition for all classes of products, Class 1, 2, 3,. The issue being, if the boards are hot air leveled and there is exposed copper means that non wetting is occurring and this is not acceptable. The basis material is exposed and it is not supposed to be exposed. IPC-A-610, the assembly document states in sect 6.5.6 Nonwetting that this is a defect for Class 1, 2, 3, if solder is required. Since this board is HAL, solder is required and therefore it again does not meet the requirements of the specification. So my opinion at this point is that the board is rejectable. Now for the reality. Exposed copper will not cause you a problem, many products have been built through the years with exposed copper, if not on the ends of the component leads, along the edges of all the conductor traces. And by the way go check your plumbing in your house and let me know how your copper pipes are doing after all these years. We also have boards that are OSP protected, once these boards are soldered the OSP coating is for all practical purposes gone, so you have exposed copper all over the board if the solder did not wet to the edges of all the pads. Some companies have been building boards like this for over 20 to 25 years. What to do? Identify the condition as a defect due to it does not meet the specification, work with your subcontractors to get their act together, and disposition the boards to use as is. That's my cut at it. Will be interested to hear what others have to say. Leo Lambert Technical Director EPTAC Corp [log in to unmask] www.eptac.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Mario Dion Sent: Thursday, November 06, 2003 5:10 PM To: [log in to unmask] Subject: [TN] Assembled pcb with exposed copper; is conf.coating appropriate to "isolate" the exposed copper ? Bonjour Technetters, Would a pcb assembly with exposed copper around some vias be reliable if fully coated with conformal coating so copper won't be exposed anymore ? The problem was not detected at the incoming inspection so many pcb were assembled. Board finish is HASL. Thanks for your comments, Salutations, ___________________________ Mario Dion, T.Sc.A./ A.Sc.T. Production Engineering Mediatrix Telecom Inc. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------