--------------------------------------------------------Original Message-----
From: Ingemar Hernefjord (KC/EMW) [mailto:[log in to unmask]]
Sent: Wednesday, October 29, 2003 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Phosphorous in epoxy moldsGosh, you mean I'll be talking to the walls...walls..walls...walls.../Inge--------------------------------------------------------Original Message-----Inge,
From: David Douthit [mailto:[log in to unmask]]
Sent: den 29 oktober 2003 13:48
To: TechNet E-Mail Forum.; Ingemar Hernefjord (KC/EMW)
Subject: Re: [TN] Phosphorous in epoxy moldsThe molding compound was manufactured by a major Japanese company.
It was shipped world wide to anyone who wanted to buy it.Didn't seem to be a major problem to most users.
It was a serious problem for a number of computer manufacturers. The military got rather excited also!
They don't want to talk about it.David A. Douthit
Manager
LoCan LLC"Ingemar Hernefjord (KC/EMW)" wrote:
Nikkei, CALCE and others warned for red P particles in IC plastic packages. Could cause migration between terminals and electrical failures.This was last year. Didn't seem to be a major problem to most users. Anyone who knows if such P 'doped' molds were used by tantalum cap makers too?Ingemar Hernefjord
Ericsson Microwave Systems---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------