I think you talking about chromate conversion coating
Aleks
----- Original Message -----
From: [log in to unmask] href="mailto:[log in to unmask]">Steve Kelly
To: [log in to unmask] href="mailto:[log in to unmask]">[log in to unmask]
Sent: Thursday, October 02, 2003 5:34 PM
Subject: Re: [TN] Anti-tarnish on copper

I am not asking to put this on – I am asking when we receive raw material from our supplier what has the copper manufacturer put on ( i.e. Sommers or Gould or Mitsui as examples of copper suppliers) . Regards Steve Kelly

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, October 02, 2003 5:19 PM
To: [log in to unmask]
Subject: Re: [TN] Anti-tarnish on copper

 

Hi Steve!

I could be wrong, but I think that might be another name for OSP, Organic Solder Preservative...

-Steve Gregory-


Does anyone know what is in anti-tarnish? Is there a specification on thickness or composition? Thanks .



Steve Kelly



PFC Flexible Circuits Limited

Ph: (416) 750-8433

Fax: (416) 750-0016

Cell: (416) 577-8433

E-Mail: [log in to unmask]



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------