Mike, Kapton (polimide) tape with acrylic adhesive takes 250-300°C for a very long time. High enough? Does it have to be removable afterwards? If not, how about a non-conductive adhesive? Steve Creswick - Gentex Corporation -----Original Message----- From: Mike Wolf [mailto:[log in to unmask]] Sent: Wednesday, October 15, 2003 8:35 AM To: [log in to unmask] Subject: [TN] High temp soldermask? Can anyone suggest a soldermask capable of withstanding high (substantially higher than reflow) temperatures? Michael Wolf EH&S Manager EVI Technology LLC 7138 Columbia Gateway Drive Columbia MD 21046 Phone # 443-542-0127 Fax # 410-290-1925 [log in to unmask] www.evitechnology.com --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------