Howard: It depends on the complexity of the board. It could be 0.7, 1.9 or 3.5. One board can have two defects others can have 7 defects and some none. DPU is a defect average of many boards of the same type. DPUs can be compared with other groups of boards of the same type. Gauging the whole shop for quality, a better method can be used, which is DPMO. Using DPMO all the boards can be put in the metric. Every part that gets placed by the chip shooter or the pick and place, every solder joint are opportunities. A DPMO of under 1000 is a good number in my point of view. Under 500 is great. Regards, Ramon > -----Original Message----- > From: Howard Watson [SMTP:[log in to unmask]] > Sent: Wednesday, October 01, 2003 5:22 PM > To: [log in to unmask] > Subject: [TN] DPU and PPM > > > Hi everyone, > > The upper management team here uses a DPU metric for our board shop, for > what reason I am trying to comprehend. Basically, one solder joint defect > on a board equates to the whole board counting as a defect. The > opportunities are irrelevant - every board gets one opportunity. When the > "PPM" numbers are published, which is what they call them, they are > outrageously high. My questions are: > Does anyone use Defects per Unit at the board level? > If so, what kind of numbers are you seeing.? > > I am pursuing a change to use real DPMO metrics, but so far I've been > unsuccessful. I even presented IPC-7912, but it was ignored. Thanks in > advance for the help. > > Howard Watson > SMT Manufacturing Engineer > AMETEK/Dixson > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > Grand Junction, CO --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------