Adam: Is it possible to rotate panels to be etched 90 deg every some many seconds? This way the chemical will not run down and etch more metal towards the bottom side. a thought Regards, Ramon > -----Original Message----- > From: Rudy Sedlak [SMTP:[log in to unmask]] > Sent: Wednesday, October 01, 2003 9:55 AM > To: [log in to unmask] > Subject: Re: [TN] spray nozzle configuration for etching > > There was an excellent paper delivered at the IPC meeting in California > this last spring discussing this subject.... > > And, to cut to the heart of it....the answer it gave to your question was, > in essence, "it depends on how the nozzles are placed"... > > Wish there was a simple answer.... > > Rudy Sedlak > RD Chemical Company > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------