Correction !
Pitch  > 1.25 mm pitch shall not encroach both sides of the land or exceed  0.05 mm 
Pitch  < 1.25 mm pitch shall not encroach both sides of the land or exceed 0.01 mm
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Wednesday, September 24, 2003 4:23 PM
To: [log in to unmask]
Subject: Re: [TN] Silkscreen in solder pad

Yes, there is. IPC-A-600  2.9.3 
I am sure this requirement is also reflected in IPC-6012A
Solder Resist on other conductive patterns (SMT land patterns included) 
< 1.25 mm pitch shall not encroach both sides of the land or exceed  0.05 mm 
> 1.25 mm pitch shall not encroach both sides of the land or exceed 0.01 mm
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of West, Jim
Sent: Wednesday, September 24, 2003 3:33 PM
To: [log in to unmask]
Subject: [TN] Silkscreen in solder pad

Hi,
 
Is there a IPC standard for how much, if any silkscreen can overlap a solder pad?  What process is recommended for cleaning a solder pad with silkscreen overtop of it?  Examples I have are silkscreen on 0805 pads halfway through it, and some with silkscreen just barely touching.
 
Thanks,
Jim
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------