Yes,
there is. IPC-A-600 2.9.3
I am
sure this requirement is also reflected in IPC-6012A
Solder
Resist on other conductive patterns (SMT land patterns included)
<
1.25 mm pitch shall not encroach both sides of the land or exceed 0.05
mm
>
1.25 mm pitch shall not encroach both sides of the land or exceed 0.01 mm
Hi,
Is there a IPC
standard for how much, if any silkscreen can overlap a solder pad? What
process is recommended for cleaning a solder pad with silkscreen overtop of
it? Examples I have are silkscreen on 0805 pads halfway through it,
and some with silkscreen just barely touching.
Thanks,
Jim