Paul has hit it on the head. Particularly with solder pastes, they mostly absorb humidity like a sponge and this affects the printing, as well as the soldering. Keep stencil open times as short as possible. With liquid fluxes, the effect should be less remarkable but if you use an air driven spray fluxer or a foam fluxer, the extra humidity in the air, especially if compressed, could certainly effect alcohol-based "no-clean" fluxes. Brian Howard Watson wrote: > > Hi all, > > There is a presumption (not supported with data) here that when it > rains, and the humidity goes up, we historically have experienced more > solder defects. I realize that humidity can affect MSD's and PCB's, but > what, if any, would be the symptom of high humidity, in terms of solder > joint defects at wave and reflow (solder balls,voids)? Our process is > strictly no-clean. Normally, the humidity in our plant is 10-30%, and > when it is high, it's in the 50-60% range, which is probably not even > that high compared to some of your plants located in humid climates. I > suspect that our problem may be something other than the humidity. > > Also, we don't bake our PCB's, and I'm not sure if it's necessary. > > Howard Watson > SMT Manufacturing Engineer > AMETEK/Dixson --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text > in the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site > http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- > > Grand Juction, CO --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------