Message
BACKGROUND:
On one assembly, we
use semi-automatic air displacement paste dot dispensing and a semi-automatic
placement system. The computer says where to put the paste and parts, the
operator places them by eye in the correct location. With normal accuracy, we
get a few solder balls that squeeze out from under the chips at the
side which are easy to pick off. Recently, we got a batch that have lots of
solder balls trapped under the middle of the parts. It was a newly trained
operator that built these assemblies.
QUESTION:
What is the most
likely cause?
What is the best way to rework
a chip part with a solder ball under the
middle?
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------