You
can test Au hardness on ceramic substrates but I've never had much success doing
hardness testing of Au/Ni/Cu on epoxy glass laminate boards. Background
substrates are to soft and inconsistent to get reliable/repeatable readings or
meaningful results.
Regards,
Bruce
Misner
Hi all,
I have 2 questions for
electroplated soft gold.
1) Recommendations on reliable outside
service
2) Is anyone doing hardness test on circuit brd itself.
How reliable is that ?
Thanks in advance.
Rashesh
---------------------------------------------------
Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e
To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of
previous posts at: http://listserv.ipc.org/archives
Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------