You can test Au hardness on ceramic substrates but I've never had much success doing hardness testing of Au/Ni/Cu on epoxy glass laminate boards. Background substrates are to soft and inconsistent to get reliable/repeatable readings or meaningful results. Regards, Bruce Misner -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, September 02, 2003 2:04 PM To: [log in to unmask] Subject: [TN] Questions on Soft gold plating. Hi all, I have 2 questions for electroplated soft gold. 1) Recommendations on reliable outside service 2) Is anyone doing hardness test on circuit brd itself. How reliable is that ? Thanks in advance. Rashesh --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------