I should have been more clear. How much can a PCB bend without damage? I have seen 4 and 3 point tests described, but no details. I already no about the bow and twist measurements, but I need to actually bend the boards and determine their stiffness and damage resistance. Paul Stolar Materials Engineer Houston Technology Center Baker Atlas 713-625-5376 713-625-4949 (fax) -----Original Message----- From: Chris Robertson [mailto:[log in to unmask]] Sent: Monday, August 18, 2003 1:34 PM To: TechNet E-Mail Forum.; Stolar, Paul W Subject: Re: [TN] FW: Bend test Bend test? For what reasons. There is a bow test... Chris Robertson [log in to unmask] ----- Original Message ----- From: Stolar, Paul W <mailto:[log in to unmask]> To: [log in to unmask] Sent: Monday, August 18, 2003 1:04 PM Subject: [TN] FW: Bend test Is there an industry standard bend test? I have found many people doing them, but no standard. Paul Stolar Materials Engineer Houston Technology Center Baker Atlas 713-625-5376 713-625-4949 (fax) --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------