What is the best etchant to use for small scale high density copper
nickel gold pattern plating line?
Not trying to be "a wisea...", but what you mean by "best" etchant? Suspect you may be limited to ammoniacal because of exposed Nickle on edges.
Rudy Sedlak
RD Chemical Company