Wee Mei, We also had a case where a pink poly had an amine in it and one of our employees broke out in a horrible rash - to the point where she was taken to the hospital. regards, Bev Christian Research in Motion -----Original Message----- From: Lum Wee Mei [mailto:[log in to unmask]] Sent: August 27, 2003 3:47 AM To: [log in to unmask] Subject: [TN] ESD Pink Bubble Wrap/Bags Hello, We recently ordered cushioned ESD bags and a big roll of the pink bubble wrap. The pink bubble wrap is used to wrap PWBA that are bigger than those ESD bags that we ordered. I have heard that pink bubble bags have impact on PWBA even though they are ESD. However, my supplier ensure that there is no problem or impacts at all as long as they are ESD coated. I just came back from the IPC-A-600 Inspector course and was told by my instructor that pink bubble bags absorb moisture readily and will age the PWBA ESD coated or not as it produce dioxin. This will cause the PWBs difficulty in wetting. I just searched the TechnNet archieves but I am lost in those messages. Can someone be kind enough to give me some good reference or advice what am I going to do with that big roll of pink bubble wrap? Thanks and regards, Wee Mei --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------