Kay Thanks for this explanation. But is it not a dangerous distinction? TBBPA is, as far as I'm aware, used only where TBPA is part of the prepolymer formulation, namely in epoxy resins and polycarbonates. What is used in other laminates, such as polyimides? Why is there such a fuss about bromine-free laminates if there is no political pressure? If it is just a "green" action (IMHO, justified), then why is TBBPA excluded, when we do have non-brominated substitutes already available? I'm just perplexed why a probably environmentally favourable action (Br-free laminates), with scientific backing, should be pooh-poohed by the IPC when it actively promotes an environmentally unfavourable action (Pb-free solder) without a scrap of scientific evidence as to the sustainability. Brian Kay Nimmo wrote: > Dear Brian > > It is quite simple - both articles are correct. > > RoHS does not currently apply to all brominated flame retardants, only to PBB and PBDE. These are typically used in plastic housings etc. TBBPA used in laminates is not covered by RoHS. > regards > Kay > > -----Original Message----- > From: Brian Ellis [mailto:[log in to unmask]] > Sent: 21 August 2003 12:15 > To: [log in to unmask] > Subject: [LF] WEEE/RoHS clarification required > > > I've just received the August IPC Review. > > On p. 6, there is an article, "Lead Time on Lead Free Dwindles". This > re-states the deadline of 1 July 2006 for total lead-free soldering for > products sold in Europe (ignoring the few named exceptions). > > On p. 4, there is an article, "IPC Quells Flames of Halogen-Free Issue", > which claims, after study, that there is no reason not to use > halogenated flame retardants, such as TBBPA. > > It is my understanding that the same EU directives require all laminates > and plastics in electronics assemblies to use non-halogenated flame > retardants, presumably from the same date (I have not checked this in > the actual directives). > > Does this not reveal an extremely dichotomous polity on the part of the > IPC? On the one hand, the IPC has gone hell-for-leather towards the > lead-free goal, without an ounce of proven scientific reason. On the > other hand, the IPC is opposing the halogen-free part of the same EU > legislation, despite the fact that emissions of incinerated > halogen-containing laminates may contain some highly hazardous and > polluting substances, as shown by scientific studies. At the same time, > it may lull exporters to the EU and members within the EU into a false > sense of security into thinking that brominated flame retardants are > here to stay, rather than be mandatorily substituted within a few years. > > I need clarification on this paradoxical dichotomy. > > Brian > > -------------------------------------------------------------------------------Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Leadfree > To temporarily stop delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL > Search previous postings at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ------------------------------------------------------------------------------- > > ----------------------------------------------------------------------------------------------------------------- > Tin Technology Ltd & ITRI Limited > Unit 3, Curo Park > Frogmore > St Albans > Hertfordshire, AL2 2DD > > Phone number: +44 (0)870 458 4242 > Fax number: +44 (0)870 458 4273 > www.tintechnology.com > ----------------------------------------------------------------------------------------------------------------- > > This information given in this e-mail is for guidance only. It should be reproduced only in full, with no part taken out of context without prior permission. We believe the information provided in this statement and any attachments is reliable and useful, but it is furnished without warranty of any kind from the authors. > Potential users should make their own determination of the suitability of any information provided and adopt any safety, health, and other precautions as may be deemed necessary by the user. > No licence under any patent or other propriety rights is granted or to be inferred from the provision of the information herein. In no event will Tin Technology or any of its affiliates be liable for any damages whatsoever resulting from the use of or reliance upon this information. > > The information contained in this e-mail is intended only for the individual or entity to whom it is addressed. It may contain privileged and confidential information and if you are not an intended recipient you must not copy, distribute or take any action in reliance on it. > If you have received this e-mail in error, please notify us immediately by telephone on +44 (0)870 458 4242. Please also destroy and delete the message from your computer. > > > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------