Soft water is not DI water, [although DI water is soft.] You can make hard water soft by adding salts to it , for example washing soda -sodium carbonate. Naturally the water is now full of ions, but not the ones which interfere with the action of soaps /detergents. Deionised water is what it says, pure water, H2O and nothing else. Naturally it is soft as it has nothing in it to interfere with soaps etc that would make it hard. So yes you can use softened water as an intermediate rinse, but clearly water softened as above will leave the dissolved salts on your work if used in the final rinse. The reason for using softened water is that it usually much cheaper than DI water. Regards Mike Fenner Applications Engineer, European Operations Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Pb-free: www.Pb-Free.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Macko, Joe @ IEC Sent: Wednesday, August 20, 2003 12:02 AM To: [log in to unmask] Subject: [TN] water soluble flux in line cleaner water wash Fellow Techies, Hopefully, someone can shed some light on my concern about rinsing boards (soldered with water soluble flux) with softened water vs. DI water. A board assembly house suggested that it is acceptable to do in-process rinsing using "softened" water (in an in-line cleaner) and save the "DI water" rinse for the FINAL in-line cleaning. In-process cleaning would be for example after the 1st side is soldered on a double sided board. Seems like a lot of extra work to me switching from softened to DI water. Look forward to your comments. thanks joe ::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::: This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice. ::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::: --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------