Don, You didn't say where the rework was needed. If the rework is in the epoxy, based upon the methods suggested, it sounds like the hardware being worked on will be compromised to some extent. If the rework is outside the potting (e.g.. wires too short), then I might suggest using a crimp splice covered with shrink tubing, The crimps could be staggered so that the overall wire bundle size would remain about the same. Of course what ever documentation you need to provide to deviate from the print must be mutually agreed to by all parties. Bill Kasprzak Moog Inc, Electronics Process Engineering -----Original Message----- From: Donald Vischulis [mailto:[log in to unmask]] Sent: Tuesday, August 05, 2003 2:05 PM To: [log in to unmask] Subject: [TN] Epoxy Removal I need some quick suggestions. I have a sensor assembly (metal body) with epoxy potting covering a header and wire terminations. The termination area is potted in epoxy, and the volume is about the size of a sewing thimble. The wires require rework. Is there a way to remove the epoxy to get to the wire terminations? Any and all suggestions appreciated. Don Vischulis --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------