I am probably
not alone in feeling twitchy about this, if the solvent you are using does not
run off the board then really you haven't removed anything, but dispersed
it so you or your customer can't see it.
I suppose you
could say it has been absorbed by the pen, but If it has been absorbed by the
pen it is just put back down in increasing concentrations each time you use the
pen....
Or you could
argue that as the assembly works the residues must be dispersed enough so
that the amount per area is below some critical point and therefore no
longer a hazard.
I suppose if
the customer specifies it and/or is happy with product reliability then it
is OK, but I still feel twitchy.
Regards
Mike Fenner
Applications
Engineer, European Operations
Indium Corporation
T: +
44 1908 580 400
M: + 44 7810 526 317
F: +
44 1908 580 411
E: [log in to unmask]
W:
www.indium.com
Pb-free:
www.Pb-Free.com
Jim,
Sorry for not explaining. The Pad
Prep Pen is used for rework, particularly with our hot air rework station.
When removing the component, flux is applied to the leads. After
component removal, the flux residues are then cleaned off the pads, to prepare
the pads for soldering the new component to the board.
Howard Watson
SMT Manufacturing
Engineer
AMETEK/Dixson
Howard:
I can't help asking: why do you remove no clean flux
residues?
Jim Smith
Managing Director
Electronics Manufacturing
Sciences, Inc.
4285 45th St. S.
St. Petersburg, FL 33711-4431
Tel:
(727)866-6502 ext. 21
Fax: (727)867-7890
eMail: [log in to unmask]
Howard Watson wrote:
Jim,
Interesting that you ask, as I was just in the
process of ordering some more of the pens that we use, which is called a "Pad
Prep Pen", made by A.P.E. , P/N is 8200-1350, 8 for $89. I don't have
experience with any others, so I won't place judgement. However, our
operators love this one for removing our no-clean flux residue.
Howard Watson
SMT Manufacturing
Engineer
AMETEK/Dixson
Good afternoon,
I
was informed by my purchasing department that Multicore (part # MC-PV-01) is no
longer making their Mini-cleaner (prozone pen), that we were using to remove
flux residue from hand soldered applications. We have received a sample
from a different supplier that is supposed to do the same thing, the only
problem is the pen leaks severely when you push on the tip. This may be a
bad sample, but we are not off to a good start trying to find a replacement.
Does anyone else out there use these types of pens to remove flux residue
from hand soldering or similar applications? If so, what manufacturer do
you use and how do the pens perform? You can email me off-line if you
like.
Thanks,
Jim West
---------------------------------------------------
Technet Mail
List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe,
send a message to [log in to unmask] with following text in the BODY (NOT the subject
field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet
send e-mail to [log in to unmask]:
SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts:
send e-mail to [log in to unmask]:
SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach
Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail
List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe,
send a message to [log in to unmask] with following text in the BODY (NOT the subject
field): SIGNOFF Technet
To
temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts:
send e-mail to [log in to unmask]:
SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach
Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List
provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a
message to [log in to unmask] with following text in the BODY (NOT the subject
field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet
send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE
mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet
Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact Keach
Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------