Technetters,
As if
we didn't have enough problems with really, really old parts; part numbers;
moisture sensitivity; a few instances of stupid finishes as suppliers go
lead free; but now I have a new one - for me anyways. We have received
virgin parts where the label on the bag says they only have a SOLDERABILITY
LIFETIME of 168 hours after they are taken out of the bag! This is not a
case where one can recover them by putting them in an oven afterwards!
Anyone else seeing this new pain-in-the-neck development?
regards,
Bev
Christian
Research in Motion