To: [log in to unmask]
Subject: Re: [TN] High temp pastes for wave soldering...Getting the paste isn't too hard. But, reflow (25-40 degrees above liquidous) temperature for those alloys is hazardous for FR-4, and many components. Ceramic chip caps and thick film resistors might be okay but this is clearly over the top for most plastic IC packages. We have done some experimenting with direct attach and forming-gas to ceramic using these alloys. One day we ran an FR-4 board though the oven without thinking. What came out of the oven would best be described as ash with body.--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------------------------------------------Original Message-----Hi Steve,
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, September 06, 2002 3:20 PM
To: [log in to unmask]
Subject: Re: [TN] High temp pastes for wave soldering...
Hope you don't mind, I put a subject in the subject box for your post...
As far as through-put issues with your dispenser, why not print your epoxy. You would do the whole board in well less than 30-seconds, and have much better accuracy and consistency than you could ever expect from a dispenser.
As far as high temperature pastes go, you would need one of the high-lead alloys in order to be above the typical solder pot temperature of 500° F (260° C). Getting these alloys in paste form is going to be challenge as well, you can bet that it's going to be a custom order with a minimum buy too.
A few of those alloys are:
° F ° C
Sn10Pb90 514 - 576 268 - 302
Sn10Pb88Ag02 514 - 570 268 - 299
Sn05Pb92.5 Ag2.5 536 280
My two-cents...
-Steve Gregory-
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------