MessageSo far as I understand it the EU directive exempts solders with more than 90% lead content from the Pb ban, This is in recognition of the fact that for high temperature soldering there is no real alternative . The exemption is primarily aimed at power die attach and similar applications. High leads are available in paste presentations, and represent somewhat of a challenge to use in most areas. (but are used routinely in SMT /hybrid thick film assembly as well as the more "traditional" areas of device manufacture). For example peak reflow temperatures are high at over 300C -sometimes 350C so getting there with minimal delta T is tough on regular SMT equipment. Most organic materials and certainly some flux resins are at or beyond performance envelope and so need careful selection, and so on. Nitrogen reflow is advised to reduce oxidative degradation and ease cleaning. Regards Mike Fenner Applications Engineer, European Operations Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Pb-free: www.Pb-Free.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Dave Chapman Sent: Tuesday, July 15, 2003 3:39 PM To: [log in to unmask] Subject: Re: [TN] High temp pastes for wave soldering... Is there an exemption from Lead Free requirements for solder paste? And is that also the case for wave soldering PCBs? Dave Chapman -----Original Message----- From: Guy Ramsey [mailto:[log in to unmask]] Sent: Friday, September 06, 2002 3:14 PM To: [log in to unmask] Subject: Re: [TN] High temp pastes for wave soldering... Getting the paste isn't too hard. But, reflow (25-40 degrees above liquidous) temperature for those alloys is hazardous for FR-4, and many components. Ceramic chip caps and thick film resistors might be okay but this is clearly over the top for most plastic IC packages. We have done some experimenting with direct attach and forming-gas to ceramic using these alloys. One day we ran an FR-4 board though the oven without thinking. What came out of the oven would best be described as ash with body. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Friday, September 06, 2002 3:20 PM To: [log in to unmask] Subject: Re: [TN] High temp pastes for wave soldering... Hi Steve, Hope you don't mind, I put a subject in the subject box for your post... As far as through-put issues with your dispenser, why not print your epoxy. You would do the whole board in well less than 30-seconds, and have much better accuracy and consistency than you could ever expect from a dispenser. As far as high temperature pastes go, you would need one of the high-lead alloys in order to be above the typical solder pot temperature of 500° F (260° C). Getting these alloys in paste form is going to be challenge as well, you can bet that it's going to be a custom order with a minimum buy too. A few of those alloys are: ° F ° C Sn10Pb90 514 - 576 268 - 302 Sn10Pb88Ag02 514 - 570 268 - 299 Sn05Pb92.5 Ag2.5 536 280 My two-cents... -Steve Gregory- ------------------------------------------------------------------------ --------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ------------------------------------------------------------------- -------------- -------------------------------------------------------------------------- ------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ------------------------------------------------------------------- -------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- ::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::: This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice. ::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::: --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------