Rich, The part A and B may be degassed prior to shipping. Once you open the package, you may introduce the gas into the system. jk -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Rich Lasko Sent: Thursday, July 10, 2003 11:05 AM To: [log in to unmask] Subject: Re: [TN] Potting Problems Storage temperature is approx. 72 degrees F. The components (part A & B) are stored in the same location and same temperature. And each time we begin using the product it works great. But after a few days, we have bubbles. Rich -----Original Message----- From: Rudy Sedlak [mailto:[log in to unmask]] Sent: Thursday, July 10, 2003 9:43 AM To: [log in to unmask] Subject: Re: [TN] Potting Problems What is the storage temperature? Have you tried storing the components of the potting mix in the same area (same temperature) in sealed containers, so that you can determine if the problem is inherent in the chemistry, or has to do with the dispensing apparatus? Rudy Sedlak RD Chemical Company --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------