Hi Frank, Funny, these pictures look just like some of my own. If you have established that all of your processes are in order, then check the board itself. Check to see if the board will take solder in these locations with an iron. If no, as it was in my case, then check other boards in this lot to see if you have an issue in the same ref designated areas. If you do, then your board manufacture may have had a process issue with the plating or cleanliness. You will need to investigate a cross section of the suspect solder joint and see what is going on. In my case, it turned out to be a poor tin/nickel plating process which resulted in a phenomena called "Black Pad". http://www.omg- galvano.com/pdfs/VeroeffentlichungenEnglisch/GT_2281_2286.pdf. This, in a nutshell, is hyper oxidation which can be caused by several factors. Ours has turned out to be poor plating (nickel layer was too thin) by the board manufacture. I don't claim to know anything about this phenomena however, as I understand it, the causes can be: 1. poor plating processes (nickel layer too thin)! 2. oxidation through the gold layer (thin porus gold can allow oxidation) 3. Excessive heat cycles (clean and bake, smt cycles prior to wave???) 4. Pre cleaning chemistry accelerating oxidation 5. Copper contamination or phosphorous content. Keep in mind, if all of your other boards are going through your process without this problem, the issue is likely with your board supplier. Good luck --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------