Hi Technetters; This inquiry is really aimed at the board manufacturers out there. I am trying to benchmark the settings for .062 thick, 170 Tg material for HASL. The unit is a QuickSilver vertical leveler. Can anyone provide the recommended settings for: a) insert speed b) withdraw speed c) air-knife temperatures d) air-knife pressures Thanks, --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- Rob