Subject: [TN] Underfilling BGA components
Does anybody have data and experience with the improvement or degradation in reliability by underfilling a cavity down, 1 mm BGA pitch, PBGA package? The PCB thickness in this situation would be greater than 0.110.
Thanks.
Stephen Ayotte, IMD Manufacturing Quality Senior Engineer
Dept. N62V, Bldg. 966-2, Office 2J1309, Mail Drop 967A
Phone (802) 769-4775, t/l 446-4775, Fax (802) 769-4139
Pager (802) 878-5386 Pin #4685 - external, 74685 - internal
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------