There are more than one way to secure the TC on the board. In some cases the boards are very expensive and scraping one is not an option. Based on posts on the list and personal experience the best way is using higher temperature than eutectic solder to secure the TC.. Another way is using Kapton tape. If you are careful and run a board, after it has been reflowed and cooled off, a second time with the TC attached at the places of interest, a very close representation of the profile will result. It is important that the TC do lay flay on their own on the board. In other words form them so they stay on the board without having to force them down on the board. The Kapton tape gets soft with heat and the adhesion gets weakened. If there is any springing on the TC, the TC will win and it will pull away from the board. The thermocouples wires have to be routed so they will not interfere with components, specially BGA. Since everything will reflow again, It is very important that all wires stay clear of components and not move them. Either way kapton or high temp solder, it is easier if you run a board that has all the parts reflowed and has cooled off, this way you don't have to worry about disturbing parts as you place the TCs. As long as you run the board only two times is still usable. Regards, Ramon > -----Original Message----- > From: McCall,Doug [SMTP:[log in to unmask]] > Sent: Tuesday, July 29, 2003 3:34 AM > To: [log in to unmask] > Subject: [TN] Attaching mole thermocouples to PCBA's being profiled > at reflow > > Hi all, > > When profiling a PCB assembly through a reflow oven process > how do you guys actually attach the thermocouples. The reason > for asking this question is that if you attempt to put the wires > (x6) over the wet solder paste then the components & devices will > be moved by the loose thermocouple wires. > > Therefore, I have been using a scrap PCB assembly and profiling a > number of times, but this means having a scrap one out of the batch. > > Any thoughts appreciated. > > Thanks, > > Douglas I McCall, > PCB Manufacturing Engineer > > BOC EDWARDS, > Marshall Road, > Eastbourne, > East Sussex, > BN22 9BA UK > Tel: +44 (0) 1323 501 147 > Fax: +44 (0) 1323 509 824 > mailto:[log in to unmask] > > > _____________________________________________________________________ > This e-mail has been scanned for viruses by MCI's Internet Managed > Scanning Services - powered by MessageLabs. For further information visit > http://www.mci.com > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------