One issue you need to address is volume. My wave is used about once every week. We waste a lot of flux using a foam fluxer.  You would not waste as much with a sprayer.

 

Nitrogen is very important. It improves yield and reduces dross.

 

I don’t know about the air knife.  Mine does not have one.

 

Paul Stolar

Materials Engineer

Houston Technology Center

Baker Atlas

713-625-5376

713-625-4949 (fax)

-----Original Message-----
From: Fred Pescitelli [mailto:[log in to unmask]]
Sent: Friday, June 20, 2003 1:54 PM
To: [log in to unmask]
Subject: [TN] Wave solder

 

I am investigating used wave solder equipment. How important is spray fluxing versus foam fluxing, also how important is it that the unit have a hot air knife, and be nitrogen capable. We will only be using it for assorted thru hole components on mostly surface mount boards that have been already refolded. I don't anticipate doing any wave soldering of SMD components.

 

Thanks,

 

Fred

 

Fred Pescitelli C.I.D.
Phoenix Designs
4057 Darling Ct.
Lilburn, GA  30047
Mailto:[log in to unmask]
http://www.phoenixdesigns.com
Office:  770-923-3465
Cell:  404-405-7668
Fax:  770-923-2272

 

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
-----------------------------------------------------