Carl, I would recommend immersion silver. Regards, George George M. Wenger Andrew Corporation 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [log in to unmask] -----Original Message----- From: Carlr Ray [mailto:[log in to unmask]] Sent: Monday, June 09, 2003 6:32 PM To: [log in to unmask] Subject: [TN] LCC HASL and Immersion Silver Hello All, Got a question for you guys.... I have a customer who has a product in design review. We provided feedback with the following concerns. My question is what would you guys recommend for an alternative surface finish if the customer does not change parts? 1. PCB has 3 FPBGAs, 1.0 mm pitch (64 ball count) 12mm x 14mm package 2. PCB has 1 LCC, .5mm pitch (28 pins) 10mm x 10mm package 3. PCB has 4 QFPs, <.5mm pitch (28 - 204 pin count) 4. PCB has HASL finish We have recommended changing the LCC to a BGA or QFP device and changing the finish to Immersion Silver. Carl Ray Sr. Manufacturing Engineer Huntsville, AL 35807 Phone: 256-882-4800 ext. 8845 Cell: 256-990-1990 --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- ------------------------------------------------------------------------------------------------ This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ------------------------------------------------------------------------------------------------ [mf2] --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------