Could be the softening point of the new plastics/polymers is different to the old. [Softening point is described on data sheets as glass transition temperature or Tg]. Alternatively the properties above the Tg are markedly different. Mechanical properties of polymers above the Tg are usually not documented at all, This is an easy overlook when looking at functionality of materials. Above Tg things like strength and expansion coefficients are different. I'm tempted also to suggest opaque covers...... :) Regards Mike Fenner Applications Engineer, European Operations Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Pb-free: www.Pb-Free.com -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Rick Thompson Sent: Thursday, June 05, 2003 2:30 PM To: [log in to unmask] Subject: Re: [TN] Wave Solder Advice? Peter, Thanks for the feedback. We did find out from the vendor after a couple of months of going back and forth on the issues that they had made what they consider 'minor' changes to both the epoxy used to seal the relays and the case/base materials as well. Unfortunately, after getting them to get make us sample runs of the old configuration (another couple of months), we've found similar problems with those parts as well. Venting is one thing we haven't checked yet. We'll be checking it this week. Regards, Rick Thompson Sr. SMT Process Engineer SMTEK International, Inc. +1 (805) 532-2800 [log in to unmask] -----Original Message----- From: peter tremewen [mailto:[log in to unmask]] Sent: Wednesday, June 04, 2003 9:34 PM To: [log in to unmask] Subject: Re: [TN] Wave Solder Advice? Rick, Double check the setup of the wave. After we moved factories, we had unexpected trouble with the wave profiles due to the new "identical" exhaust system that was installed. It caused the preheat to be about 10 to 20 degrees cooler, just enough to put off some of our profiles. Your new instalation may be just diferant enough to cuase some unexpected or unfamilliar problems, and the relays are sensitive to this change for some reason. Like wise check that the vendor isn't spinning some "white lies", thinking that some minor change wont effect the Relay in the wave. In my limited experiance with this, some prety minor changes to manufacturing process of the components can cause some prety major headaches. Something obviously changed...... Peter T Rick Thompson wrote: > We have a board with a safety relay on it that is exhibiting moisture inside the relay case after we process it (aqueous process). After numerous discussions with the relay vendor and several rounds of testing various epoxies for sealing the case to the base of the relay, the vendor is indicating they believe our wave solder process is heating the part too much, causing expansion of the air inside and subsequent breaking of the seal. I believe our wave solder profile is fairly standard and was developed to ensure that all solder fillets on the top-side meet IPC-610 Class 3 standards. I'm hoping some of you wave solder gurus can tell me if we're way off base with our profiles. We currently aim to acheive 90-100 C on the topside of the board prior the board entering the wave. This gives us the wetting we're looking for as well as reduces the level of thermal shock on bottom side components. Is this temperature in line with what's being done in wave soldering? Is there something I should be looking at to reduce this topside temperature without sacrificing solder wetting? > > As an added note, we ran around 70,000 of these units without much evidence of this problem occurring. Our process has not changed other than to move to a new building. The vendor did change epoxy but tests with both the old and the new epoxy yield similar failure rates. --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------