Thanks for telling me that. I assume they were under cure them or just barely cure them to improve the cycle time to start with....Does that has an upper limit? (maximum 2 cure for example?) Can you send me some infor. Regarding recommended "over curing"? Many thanks. Best regards, jk (1.35 cents really) >-----Original Message----- >From: TechNet [mailto:[log in to unmask]] On Behalf Of >Robert Tarzwell >Sent: Friday, June 27, 2003 2:58 PM >To: [log in to unmask] >Subject: Re: [TN] Hysol SR1000, SR1001 - why? > > >Sorry but the industry has been adding a (short) uv bump to >lpi solder masks for years the manufactures even suggest it >for tough situations. my 5 cents worth > >--------------------------------------------------- >Technet Mail List provided as a free service by IPC using >LISTSERV 1.8e To unsubscribe, send a message to >[log in to unmask] with following text in the BODY (NOT the >subject field): SIGNOFF Technet To temporarily halt or >(re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE >mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest Search the archives of >previous posts at: http://listserv.ipc.org/archives Please >visit IPC web site http://www.ipc.org/html/forum.htm for >additional information, or contact Keach Sasamori at >[log in to unmask] or 847-509-9700 ext.5315 >----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------