Hi Ed, We have some boards here that still cost us about 10 minutes to mask off the areas that must remain clean, plus 20 minutes for manual brushing of areas that cannot be coated by our Asymtek machine. I found out the hard way that to achieve the full advantage of selective spray coating machines, it is mandatory that the boards are designed for it, including the quality requirements. Daan Terstegge Thales Communications Unclassified mail Personal Website: http://www.smtinfo.net >>> [log in to unmask] 06/05/03 07:41am >>> Asymtek/Nordson are about the best in the field. In my former slave mine, we just bought a robotic sprayer before I left for new pastures. I have to say it's great, though not cheap! It doeas away with masking/demasking and gives a beautiful, even finish. If you can justify it, go for it. Peter "Noble, Ed" <[log in to unmask]> 05/06/2003 04:39 AM Sent by: TechNet <[log in to unmask]> Please respond to "TechNet E-Mail Forum."; Please respond to "Noble, Ed" To: [log in to unmask] cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group) Subject: [TN] Conformal Coating Systems Hello All, Looking for comments regarding Conformal Coating Systems. I'm aware of several systems, seen a few, and narrowed it down to Asymtek/Nordson or PVA . We'll be dispensing HumiSeal Acrylic Materials. Would appreciate any feedback from the masses. Thank You and Appreciate Your Time, Ed Noble Process Control Supervisor<?xml:namespace prefix = o ns = "urn:schemas-microsoft-com:office:office" /> [log in to unmask] Industrial Scientific Corp. www.indsci.com voice 412.490.1884 --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- [This e-mail is confidential and may also be privileged. If you are not the intended recipient, please delete it and notify us immediately; you should not copy or use it for any purpose, nor disclose its contents to any other person. Thank you.] --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------