We started looking at electroless Ni/Pd/Au as a replacement for ENIG and pattern plate Ni/Au. Advantages seem to be solderable, wire bondable, no black pad, full trace coverage (including sidewalls), and no undercut. We still need to do our homework, but passed four of the five above. To electroplate all three makes no sense. But, if it's a replacement for ENIG, I suspect it is electroless. Glenn -----Original Message----- From: Scott Lefebvre [mailto:[log in to unmask]] Sent: Tuesday, June 24, 2003 11:52 AM To: [log in to unmask] Subject: [TN] Electro-Plated Ni/Pd/Au vs [ENIG] I have a new board shop promoting their Electro-Plated Ni/Pd/Au (hard or soft gold) surface finish over our existing [ENIG] boards. We have not had any issues with our current assemblies using [ENIG]. I am requesting any advice or information on Electro-Plated Ni/Pd/Au and if it would be worth switching to it. Any advice would be greatly appreciated, thank you in advance. SCOTT --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------