Steve, Very glad you decided to stay with us after all... My solution to the problem of saying or asking stupid things on the Technet is to keep my replies off-line whenever they are questionable (to me anyways). That way the whole group doesn't witness my ignorance. Then when I get straightened out, I can look all-knowing and wise when I post something sensible. ;-) It took several ignorant comments and questions from me before I learned, and my "filter" may still occasionally fail. We all have said at some point "I'm not going to do THAT again!", and of course, as is human nature, we do it again, and feel rotten. Being able to forgive one's self is important. Anyway, back to the question you asked, the trace definitely looks to me like it's reduced by more than 20%. What happened was either the etch resist (tin) was scratched after it was plated and before it was etched, allowing partial etching of the trace, or as you suggested, something prevented plating in that spot to begin with (like a sliver of photoresist lying on top of the trace when in went in to pattern plate). Too bad your incoming inspection missed it. Or more appropriately, that your board fab shipped it to you in the first place. Tim Reeves -----Original Message----- From: Steve Gregory [mailto:[log in to unmask]] Sent: Wednesday, May 28, 2003 10:53 AM Subject: Trace thickness problem... Hi all! I'd like your opinion on something. We're building a prototype assembly for a customer, and discovered something at final inspection that we didn't see when we received the bare fabs. We ordered 16-boards in four, 4-up panels. We found a trace that has a spot where it looks like it didn't plate up during final plating. Take a look at "Trace Thickness" at http://www.stevezeva.homestead.com There's 4-boards we've found that have this problem, 1 on one panel, and 3 on another panel, and of course they're all built up. The 6012 says that thickness can't be reduced by more than 20% of the minimum conductor thickness. I can't really tell if it's 20% or 50%. I've sent pictures both to our customer and the fab vendor. The customer wants the spot repaired, and there are a number of ways to do that. The fab vendor says it's not a problem because the stack-up drawing calls out 1-oz. copper after plating on the surface layer, and they said that there's more like 2-oz. on the surface layer, so there shouldn't be any problem, at least that's what I was told, I didn't speak to anyone directly. The stack-up is on my page too, look at "Stack-up"... The first question that comes to my mind, if 1-oz after plating was called on the stack-up, why was 2-oz plated? Or is that normal?. The drawing references our customers internal spec for fabrication, but it uses MIL-PRF-55110 for references. What are your opinions about this? Thanks everyone! -Steve Gregory- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------