Does anyone have any knowledge about Ni versus Ni/Sn plating as it relates to reliability? We cannot use pure Ni since it is magnetic. Any ideas about how thicker Pd will affect reliability? Paul Stolar Materials Engineer Houston Technology Center Baker Atlas 713-625-5376 713-625-4949 (fax) --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------