Hi All! Well, after a week of getting the bejeebers scared out of me listening to tornado warnings and watches being broadcast, sirens going off (Friday night), we've got a beautiful day here. Luckily, we didn't catch much of the really bad storms here in Tulsa... Anyway, I've just been recently informed that the R560 (water soluble), and the R244NC (no-clean) is coming off Kesters "Preferred" products. They're being replaced by a HM531 (water soluble), and a PM202 (no-clean). I'm getting samples sent to me of course, to do my own evaluations, but I was just wondering if anybody else has switched over to the new formulas, and how they like them. From a couple of discussions I have had with Kester, and reading the datasheets, these new pastes will print at faster squeegee speeds (which isn't a big deal to us since we're a low-to-medium volume shop), and wets better to different finishes, such as Ag/Pd and OSP's. The one thing that I did notice with the HM531 that I don't care for a whole lot, is that the shelf life has decreased to 4-months vs. 6-months with the R560. I can envision now, since we buy our paste through distribution, that we're going to get paste that will have very little shelf life left. We were running into that problem occasionally even with 6-month life paste. -Steve Gregory- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------