Steve,
I have soldered both type and I agree that nickel plated wire is more
difficult to "wet".
The nickel will oxidize quite rapidly and requires a more aggressive
flux and/or heat to get good "wetting".
This is particularly true for wire that has been "laying around" for
6 months or more and for the
the cut end of the wire.
You should consider pre-tining this wire before attempting repairs.
David A. Douthit
Manager
LoCan LLC
Steve Gregory wrote:
Hi All,I was posed this question by one of our customers. I don't have any experience with nickel plated wire, but it would seem to me to be difficult to solder to. I've used tin plated, and silver plated wire before with no problems. But I didn't know that silver plated wire had corrosion problems. Any inputs?
In the future we are going to be changing to specify a nickel plated wire (M22759/10-28-9) for PWA repair. The previous part number was a silver plated wire. We haven't used this before. Do you or any of your manufacturing people know of issues with solderabiliby when using a nickel plated wire or any special process that should be used?
The history of this is IPC-7721 paragraph 6.1 says silver plated wire must not be used because it can cause corrosion of wire in certain situations. Turns out that when you follow MIL-23200 the allowed wire is either silver plated or nickel plated. We would have preferred tin plated wire but it doesn't appear to fall under the allowed MIL-23200 options.
Thanks in advance!!!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------