RE: [TN] Bad laminate and warped board

Daan

You've already heard that the boards will likely warp when they go above Tg (such as during reflow).  But I'd have another concern with these.  You've already been told the material was not manufactured properly.  What assurances do you have that whatever is wrong with the material will not manifest itself in some other way.  For instance if the material is prepreg is defective because the thicknes of resin coating on the glass is uneven, what other implications, beyond warpage, does that mean in your final product?

Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------