Paul, If you're lloking for an XRF to ID plating materials and measure thickness one contact would be Fisher Technologies, 750 Marshall Phelps Road, Windsor, CT 06095, 800-243-8417 Regards, George George M. Wenger (908)-546-4531 Reliability Engineer RF Power Amplifier Group Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 [log in to unmask] -----Original Message----- From: Stolar, Paul W [mailto:[log in to unmask]] Sent: Tuesday, April 08, 2003 1:30 PM To: [log in to unmask] Subject: [TN] EDX Paul Stolar Materials Engineer Houston Technology Center Baker Atlas 713-625-5376 713-625-4949 (fax) I have used table top EDX/X-ray machines in the past to ID plating materials and thickness. But I cannot remember who makes them. Any suggestions? Paul Stolar Materials Engineer Houston Technology Center Baker Atlas 713-625-5376 713-625-4949 (fax) --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- ------------------------------------------------------------------------------------------------ This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ------------------------------------------------------------------------------------------------ --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------