Matthew
You should not have to bake boards that have been properly fabricated, properly packaged and properly stored. Your board fabricator should be able to provide you with a warranty for the boards for a specified period (they determine this, not you, but it should be about 6 months) as long as the boards are kept in the original packaging. This includes solderability and delamination.
Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263
----------
From: Gray, Matthew D HS-SNS[SMTP:[log in to unmask]]
Reply To: TechNet E-Mail Forum.;Gray, Matthew D HS-SNS
Sent: Wednesday, April 23, 2003 5:39 AM
To: [log in to unmask]
Subject: [TN]
Hello all-
I am a member of a team attempting to reduce and potentially eliminate board
conditioning (baking) for high Tg FR4 boards at our plant sites. I am
inquiring for input relating to current company trends, product basis, and
frequency of board baking prior to board assembly. The implementation of
board baking requirements were historically based on delamination frequency
at particular plant site locations - no additional failure analysis was
pursued beyond the implementation of the baking schedule being applied to
all products.
I am looking for feed back for use in a manufacturing pilot that is being
designed for a plant site that currently bakes all PWB products. Any and
all input would be appreciated for this effort.
Regards - Matt
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------