Joe, We have used cans of aerosol with the plastic tube mounted in the spray head from Chemtronics in the Flux-off Series for applications with tight clearances. Admittedly this could be expensive but you did say that you do this operation periodically. You also say that you use liquid RMA flux, I'm surprised that you haven't burned a board yet with the Air-Vac. We had an operator that made a mistake and used RMA liquid flux at the Air-Vac only to have the alcohol component burn the PC board. We use tacky flux exclusively at the Air-Vac. Hope this helps. Bill Kasprzak Moog Inc. Manufacturing Engineering, Electronics > -----Original Message----- > From: Macko, Joe @ IEC [SMTP:[log in to unmask]] > Sent: Saturday, April 26, 2003 1:57 PM > To: [log in to unmask] > Subject: [TN] cleaning under BGAs > > Fellow Technets, > > Periodically, BGAs are reflowed using our AIR-VAC hot air rework station. > RMA liquid flux is 1st flowed under the BGA prior to reflow and then clean > afterwards starting with IPA spray followed by an in-line cleaner wash. > Occasionally, flux residue remains which requires additional cleaning. > > I am in need of a creative and operator safe way to either spray/flow warm > IPA or a mixture of hot saponifier/DI water (from our in-line cleaner) > under > BGAs to expedite cleaning. I do not know of any equipment on the market > that can be used for this application. > > Welcome ALL suggestions and proven methods. thanks > > joe > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------