It would be interesting to have the information sent to the Technet. This is the alloy that NEMI recommends and a few months ago, when I tried to find it, no major paste manufacturers had it. Do they feel like moving towards this alloyÉ Regards, Ioan > -----Original Message----- > From: Gerard O'Brien [SMTP:[log in to unmask]] > Sent: Friday, March 07, 2003 11:30 AM > To: [log in to unmask] > Subject: [TN] Leadfree alloy supplier > > I am looking for a supplier of the following lead free alloy - > 95.5Sn/3.9Ag/0.6Cu. > > You can contact me off line. > > Regards > > Gerard O'Brien > Photocircuits Corporation > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------