Substates typically have anisotropic CTEs in X/Y and Z because of the effect of the glass reinforcement limiting expansion in the X/Y direction.  CB-100 is a silver filled epoxy.  Unless there is something about the size and shape of the filler and application method that would provide an orientation to the filler (I'm unaware of any of this being done with this material), CB-100 should have isotropic CTE values. 

 
Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------