All
I know all of you have headed APEX, have a drink on me. But I have a question: Is there any information on an alloy that is Sn97and Cu3?. It is proposed that the internal intermetallic formation makes it a strong solder joint for higher temperature applications. And it has also been proposed that the excess copper will lead to brittleness as the 4% gold does to solder
Phil Hinton