Tom, Re: both your scenarios, those seem sensible to me, but of course I'm somewhat biased because we take it even a step further. We use ws paste on a number of boards in SMT (they are washed prior to any pth assembly), but use nc flux in our wave solder machines. We also do any repairs or hand soldering steps downstream from wave with nc cored wire. I guess the deciding factor is that because the residues from the ws SMT process are removed, there is no combining, mixing, etc., of dissimilar flux types. -----Original Message----- From: Tom Parkinson - Quality System Manager - WinTronics, Inc. [mailto:[log in to unmask]] Sent: Tuesday, March 11, 2003 8:39 AM To: [log in to unmask] Subject: Re: [TN] Mixing fluxes - more I've read the recent questions and information concerning mixing of fluxes. I agree - do not mix flux types when soldering. However, here's one for you that can be looked at from a couple of angles.... 1. I build a board - wave solder using washable flux. Flux is activated, does it's thing, and board is soldered. 2. Water Wash and Dry the board. All washable flux residue is gone. 3. Add a couple of more components that CANNOT be washed (water will enter the component and ruin it), using NO-CLEAN. 4. Board is done. Technically, I have used 2 types of fluxes on one assembly.... Another scenario: 1. Board (described above) is finished. But, fails test - I find a bad component... 2. I have to use NO CLEAN to replace the component because I cannot water wash the board (remember the other components that cannot be subjected to water wash..) 3. Board is done. Passes test - finished. Again - Technically, I have mixed fluxes on the same assembly. In the above description, I do not see a problem - or am I missing something? Thanks, Tom --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------