Just to throw another comment in the mix on this, not knowing what components your using or functionally, but it may be that the specific component requires the pad for a closed loupe circuit internal to the component. As a rule we do not allow missing pads period. Used or not. Randy Bock Sr. Quality Manager Bryce GMS Naugatuck [log in to unmask] ----- Original Message ----- From: "Werner Engelmaier" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, March 27, 2003 9:46 AM Subject: Re: [TN] non functional pad removal > Hi Bill, > Removing non-functional lands leads to a higher propensity for resin > recession and inner-layer separation [post separation] for larger diameter > holes. Whether or not this will cause any real problems depends on the > details. > The barrel integrity is not significantly affected. > > Werner Engelmaier > Engelmaier Associates, L.C. > Electronic Packaging, Interconnection and Reliability Consulting > 7 Jasmine Run > Ormond Beach, FL 32174 USA > Phone: 904-437-8747, Fax: 904-437-8737 > E-mail: [log in to unmask], Website: www.engelmaier.com > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------