Hi Rama, I have a question to ask, do you see the paste sticking to the blades all the time, or does it seem to happen at the beginning of a run? The reason that I ask, is because I experienced this problem in the past with a paste I was using from AMT. The paste needed to be "shear-thinned", or worked, for it to perform it's best. For example, we would see the same thing you see on the first print of a run, or after lunch-break when the line sat idle for a while. The first print, if the paste wasn't "worked", wouldn't show the roll of the bead of paste in front of the squeegee that you normally want to see. When we asked about this problem with AMT, they did say that the reaology does change when the paste is more-or-less in constant motion, from what it is when sitting still for a while. If I remember correctly, some printers have a function in their programs where you can set them to "work" the paste before the print stroke...for the life of me, I can't remember exactly what they call that function...I must be going senile...hehehe Could it be that the same thing is happening with your new Kester paste? -Steve Gregory- > For more than 4 years, we were using Alpha metals, no clean 63/37 paste. > Recently we tried the Kester paste on our DEK printers. The printing > performance is far better than the Alpha Paste. So, we switched to Kester > FL250D no clean paste (63/37, 90%, Mesh -325+500 , VISC 1400-1800 ). > > But, we are having serious unexpected problem on MPM printers. The paste > does not drop from the blades after the print stroke causing big voids on > the boards. We are scrapping quite a few boards due the misprints. > > Is there any solution for this problem ? Some one suggested 'TEFLON' > coated squeegee blades. > > Sincerely, > > Rama Vemulapalli > > --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------