You might try the E-blade from Photo Stencil. It is an Electroformed Nickel blade with a very smooth surface that minimizes curtaining. William E. Coleman Vice President - Technology Photo Stencil An ISO 9001 Registered Company 4725 Centennial Blvd. Colorado Springs, CO 80919 Phone # 719-535-8528 Fax # 719-599-4334 Cell # 719-331-2433 email: [log in to unmask] <mailto:[log in to unmask]> ---------- From: Rama Vemulapalli [SMTP:[log in to unmask]] Sent: Tuesday, March 18, 2003 3:14 PM To: [log in to unmask] Subject: [TN] Squeegee blades for printers For more than 4 years, we were using Alpha metals, no clean 63/37 paste. Recently we tried the Kester paste on our DEK printers. The printing performance is far better than the Alpha Paste. So, we switched to Kester FL250D no clean paste (63/37, 90%, Mesh -325+500 , VISC 1400-1800 ). But, we are having serious unexpected problem on MPM printers. The paste does not drop from the blades after the print stroke causing big voids on the boards. We are scrapping quite a few boards due the misprints. Is there any solution for this problem ? Some one suggested 'TEFLON' coated squeegee blades. Sincerely, Rama Vemulapalli _____ Do you Yahoo!? --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- Yahoo! Platinum <http://rd.yahoo.com/platinum/evt=8162/*http://platinum.yahoo.com/splash.htm l> - Watch CBS' NCAA March Madness, live on your desktop <http://rd.yahoo.com/platinum/evt=8162/*http://platinum.yahoo.com/splash.htm l> ! --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------