Jack: Use aluminum foil to cover all parts, the void so that flux does not drip on the floor.and replace it as often as you want to. It keeps parts under the foil clean. If the accumulation is quite a bit, cut a hole in the foil and place a pan under the hole in the lowest point of the foil. It is easy and it works. You may want to line the pan with the same foil for easy cleaning. Regards, Ramon > -----Original Message----- > From: Jack Goble [SMTP:[log in to unmask]] > Sent: Thursday, March 13, 2003 3:06 PM > To: [log in to unmask] > Subject: [TN] Future 1 solder machine > > Hi, > > We have a Hollis Future one wave solder machine with a foam fluxer. When > operating the machine we tend to get a steady drip of flux off of the > entrance end of the conveyors and on to the floor. It's a pain. Is there > an easy method to prevent this that anyone has found? > > Thank you > > --------------------------------------------------- > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 > ext.5315 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------