[log in to unmask]"> [log in to unmask]">
Ervin - get yourself a copy of the
new IPC4552 specification covering ENIG. Use this document to specify the ENIG
finish for your PWB's.
Regards
Gerard O'Brien
Co-chairman of 4552
-----Original Message-----
From: Ervin Weisz
[mailto:[log in to unmask]]
Sent: Thursday, February 06, 2003
5:43 PM
To: [log in to unmask]
Subject: [TN] Evaluating ENIG
finish
Hello Everyone,
I wish to present you with an issue
that has troubled me for quite a while.
We have been ordering more and more
PCBs with ENIG finish and are generally pleased - it's flat, it solders nicely
and the products seem to be O.K.
However, on the other hand - we are
very well aware of problems associated with ENIG, i.e - the "black
pad" phenomena - solder joints cracking, components actually "popping
off" and other "goodies".
I am looking for good means
to evaluate my ENIG finished boards, before I waste a considerate amount of
money while trying to assemble them. Luckily for us, our manufacturer seems to
understand our dilemma and is very willing to cooperate with us on performing
any in-process or final test that we specify.
So, here's the catch: what do I
specify ?
Assume that you could ask for
anything (within reason, of course) - what tests would you ask your
manufacturer to perform to assure you that he will give you high quality ENIG
finish, good solderability, durable, long life solder joints, etc.?
Thank you in advance,
Yehuda E. Weisz
+(972)-3-6342045
+(972)-53-556897
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Yahoo! Mail
Plus - Powerful. Affordable. Sign up now